| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 44.1 MPa | 6400 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.48 GPa | 360 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
| Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
| 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A | |
| Dart Drop Total Energy | 53.4 J/cm @Temperature 23.0 °C |
0.100 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 178 J/cm @Temperature 23.0 °C |
0.333 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 61.0 µm/m-°C | 33.9 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 0.749 mm |
V-0 @Thickness 0.0295 in |
ALL; UL 94 |
| V-0 @Thickness 0.9804 mm |
V-0 @Thickness 0.03860 in |
All Colors |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| AAMA 303 | Pass | ASTM D4726 |
| Agency Ratings | AAMA 303 | |
| Appearance | Colors Available | |
| Automotive Specifications | CHRYSLER MS-DC28 Type B CPN3012 Color: Black | |
| GM GM7001M (PVC) | ||
| Ease of Sizing | Acceptable | |
| Features | Good Weather Resistance | |
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| PVC Cell Classification | 1-31432-33 | ASTM D4216 |
| 13344 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Applications | |
| Outdoor Applications | ||
| Profiles | ||
| Windows & Doors |