| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 53.8 MPa | 7800 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
| 4.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A | |
| 9.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
17.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A | |
| Dart Drop Total Energy | 90.3 J/cm | 0.169 ft-lb/mil | ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 59.0 °C | 138 °F | Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Features | UV Absorbing | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | General Purpose | |
| Profiles |