| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 52.7 MPa | 7640 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.68 GPa | 389 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 92.5 MPa | 13400 psi | ASTM D790 |
| Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
| Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A | |
| 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A | |
| Dart Drop Total Energy | 87.6 J/cm @Temperature 23.0 °C |
0.164 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 149 J/cm @Temperature 23.0 °C |
0.279 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 75.6 °C @Thickness 3.18 mm |
168 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Brown | |
| Features | Good Weather Resistance | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| PVC Cell Classification | 1-02453-43 | ASTM D4216 |
| 11444 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Building Materials | |
| Outdoor Applications | ||
| Profiles | ||
| Windows & Doors |