| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | ASTM D2240 |
| Tensile Strength, Yield | 50.2 MPa | 7280 psi | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 2.81 GPa | 408 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 80.3 MPa | 11600 psi | ASTM D790 |
| Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
| Izod Impact, Notched | 0.320 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
| 1.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.25 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 68.3 °C @Thickness 6.35 mm |
155 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | General Purpose | |
| Medium Flow | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications | |
| General Purpose |