| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable W3400 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | ASTM D2240 |
| Tensile Strength, Yield | 15.2 MPa | 2200 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 300 % | 300 % | Type IV, 510 mm/min; ASTM D638 |
| Tensile Modulus | 0.00758 GPa | 1.10 ksi | Type IV, 51 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 75.0 °C | 167 °F | UL Temperature Rating |
| Brittleness Temperature | -37.2 °C | -35.0 °F | ASTM D746 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
ALL; UL 94 |
| Oxygen Index | 27 % @Thickness 1.91 mm |
27 % @Thickness 0.0752 in |
ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | ASTM D149 |
| Dissipation Factor | 0.058 @Frequency 1000 Hz |
0.058 @Frequency 1000 Hz |
ASTM D150 |
| 0.058 @Frequency 1000 Hz, Temperature 30.0 °C |
0.058 @Frequency 1000 Hz, Temperature 86.0 °F |
24 hr; ASTM D150 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 188 °C | 360 - 370 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | UL QMFZ2 | |
| UL QMTT2 | ||
| Appearance | Colors Available | |
| Features | Flame Retardant | |
| Sunlight Resistant (720 hours) | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Flexible Cord Jacketing | |
| Wire & Cable Applications |