PolyOne Trilliant™ HC 5410-0030RS Natural Polyethylene, High Density (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC 5410-0030RS Natural Polyethylene, High Density (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Izod Impact, Notched 0.800 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 °C

@Thickness 3.18 mm
241 °F

@Thickness 0.125 in
Annealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 193 - 221 °C
379 - 430 °F
Mold Temperature 26.7 - 54.4 °C
80.1 - 130 °F
Descriptive Properties Value Comments
Filler / Reinforcement Glass Fiber Reinforcement
Forms Pellets
Generic Material HDPE
Generic Name Polyethylene, High Density (HDPE)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved