| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.0050
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Asia Pacific)
High heat PC/ABS blend offering high modulus / low CTE and good practical impact
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0060
cm/cm <br>@Thickness 3.17 mm
|
0.0030
-
0.0060
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Ravago Manufacturing Americas Enviramid™ N1335HL BK Post Consumer Recycle Nylon 66, 35% Glass Filled
Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D995 |
|
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced
Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4, 2577 |
|
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled
35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
|
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm <br>@Temperature 80.0 °C
|
0.0030
in/in <br>@Temperature 176 °F
|
60x60x2 mm; ISO 294-4 |
|
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm <br>@Time 86400 sec
|
0.0030
-
0.0050
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC
LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics NORYL V02570 PPE+HIPS
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.0050
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics ULTEM AR9200 PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Dry |
|
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm <br>@Thickness 3.17 mm
|
0.0030
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm <br>@Thickness 3.17 mm
|
0.0030
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm <br>@Time 86400 sec
|
0.0030
-
0.0050
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC
LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0060
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.0060
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant
Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.0070
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled
Material with 40% GF reinforcement that is used in motor insulatorsInformation provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0040
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.0040
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0060
cm/cm <br>@Time 86400 sec
|
0.0030
-
0.0060
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS
LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50
Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**)
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm <br>@Thickness 4.00 mm
|
0.0030
-
0.0050
in/in <br>@Thickness 0.157 in
|
E2P method |
|
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded
Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
|
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Conditioned, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 2577 |
|
BASF Ultramid® Seal-Fit PA6/66 (Conditioned)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | |
|
Styrolution Luran® 348 Q Transparent SAN
Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm <br>@Thickness 3.17 mm
|
0.0030
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc.
|
|||