| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | PolyOne Corporation |
| Trade Name | Trilliant™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Trilliant™ HC THC-01-AS149031 Trans Blue Acrylonitrile Butadiene Styrene (ABS).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 37.9 MPa | 5500 psi | ASTM D638 |
| Elongation at Break | 12 % | 12 % | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
| Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | <= 1.00e+12 ohm | <= 1.00e+12 ohm | ASTM D257 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Antistatic | |
| Contact Clarity | ||
| Non-Sloughing | ||
| Forms | Pellets | |
| Generic Material | ABS | |
| Generic Name | Acrylonitrile Butadiene Styrene (ABS) | |
| Processing Method | Injection Molding | |
| Regional Availability | North America | |
| RoHS Compliance | RoHS Compliant | |
| Uses | Computer Components | |
| Connectors | ||
| Electrical Housing | ||
| Electrical/Electronic Applications | ||
| Housings | ||
| Medical/Healthcare Applications |