Material Notes:
Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizers. New Product. Commercial specifications have not been established. - Flexible - Formulated without Plasticizers - High ClarityColor concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Versaflex™ CL E95. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Drying is not Required. Rear Zone = 330-370F Center Zone = 350-400F Front Zone = 360-420F Screw Speed = 100-500 RPMInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.898 g/cc
0.898 g/cc
ASTM D792
Oxygen Transmission 150 cc-mm/m²-24hr-atm
<br>@Thickness 0.120 mm,<br> Temperature 21.0 °C
381 cc-mil/100 in²-24hr-atm
<br>@Thickness 0.00472 in,<br> Temperature 69.8 °F
ASTM D3985
Oxygen Transmission Rate 1200 cc/m²/day
<br>@Thickness 0.120 mm,<br> Temperature 21.0 °C
77.3 cc/100 in²/day
<br>@Thickness 0.00472 in,<br> Temperature 69.8 °F
ASTM D3985
Viscosity 30000 cP
<br>@Shear Rate 11200 1/s,<br> Temperature 200 °C
30000 cP
<br>@Shear Rate 11200 1/s,<br> Temperature 392 °F
ASTM D3835
138000 cP
<br>@Shear Rate 1340 1/s,<br> Temperature 200 °C
138000 cP
<br>@Shear Rate 1340 1/s,<br> Temperature 392 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
10 sec; ASTM D2240
Tensile Strength at Break 17.2 MPa
<br>@Temperature 23.0 °C
2490 psi
<br>@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 11.6 MPa
<br>@Strain 100 %,<br> Temperature 23.0 °C
1680 psi
<br>@Strain 100 %,<br> Temperature 73.4 °F
Die C2 hr; ASTM D412
11.9 MPa
<br>@Strain 300 %,<br> Temperature 23.0 °C
1730 psi
<br>@Strain 300 %,<br> Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 580 %
<br>@Temperature 23.0 °C
580 %
<br>@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 126 kN/m
719 pli
ASTM D624
Compression Set 38 %
<br>@Temperature 22.0 °C,<br> Time 79200 sec
38 %
<br>@Temperature 71.6 °F,<br> Time 22.0 hour
ASTM D395B
66 %
<br>@Temperature 70.0 °C,<br> Time 79200 sec
66 %
<br>@Temperature 158 °F,<br> Time 22.0 hour
ASTM D395B
71 %
<br>@Temperature 100 °C,<br> Time 79200 sec
71 %
<br>@Temperature 212 °F,<br> Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Die Temperature 171 - 199 °C
340 - 390 °F
Melt Temperature 182 - 204 °C
360 - 399 °F
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1210
Please contact GLS Thermoplastic Elastomers for a copy of the FDA compliance letter.
ISO 10993 Part 4
ISO 10993 Part 5
USP Class VI
Appearance Clear/Transparent
Features Good Flexibility
High Clarity
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Bottles
Film
Medical/Healthcare Applications
Personal Care
Copyright © lookpolymers.com All Rights Reserved