Precision Polymer Engineering Perlast® G80S FFKM White Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G80S FFKM White Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Perlast ® G80S FFKM is a White Perfluoroelastomer 76-85 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extraction tested in accordance with United States Food and Drug Administration (FDA) requirements, Code of Federal Regulations CFR 21 § 177.2600(e,f). In July 2004, G80S gained Food Contact Notification status (FCN) from the FDA (FCN000402). Applications: All food applications. Do not use any Perlast ® grade with molten alkali metals.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
80
80
°IRHD, 0 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 11.041 MPa
1601.4 psi
-39% change after 72 hours @ 250°C; ASTM D412
18.1 MPa
2630 psi
ASTM D412
Elongation at Break 130 %
130 %
ASTM D412
143 %
143 %
10% change after 72 hours @ 250°C; ASTM D412
100% Modulus 0.01079 GPa
1.565 ksi
-35% change after 72 hours @ 250°C; ASTM D412
0.0166 GPa
2.41 ksi
ASTM D412
Compression Set 36 %
36 %
24 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 400 °C
>= 752 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 (e,f) pass
Distilled Water
pass
n-Hexane