Precision Polymer Engineering S70L Conductive Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S70L Conductive Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.Applications: Specially compounded to offer excellent physical and electrical properties over an effective temperature range of -50° to +160°C. It has good resistance to chemicals and weathering. Resistance to mineral based oils and greases is poor, but it can withstand limited splash contact.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
Tensile Strength, Yield >= 1.25 MPa
>= 181 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Compression Set 30 %
30 %
70 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flash Point >= 300 °C
>= 572 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0080 ohm-cm
<= 0.0080 ohm-cm
Mil G 83528
Shielding Effectiveness 70 dB
70 dB
@ 200 kHz; Mil Std 285
100 dB
100 dB
@ 2 GHz; Mil Std 285
100 dB
100 dB
@ 10 GHz; Mil Std 285
105 dB
105 dB
@ 500 MHz; Mil Std 285
110 dB
110 dB
@ 100 MHz; Mil Std 285