| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Armor-X™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Armor-X™ Non-Marring, Elastomer Polymeric Blend (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 50 | 50 | ASTM D2240 |
| Tensile Strength | 22.1 MPa | 3200 psi | ASTM D638 |
| Elongation at Break | 100 % | 100 % | ASTM D638 |
| Tensile Modulus | 0.355 GPa | 51.5 ksi | ASTM D638 |
| Flexural Strength | 15.2 MPa | 2200 psi | ASTM D790 |
| Flexural Modulus | 0.303 GPa | 44.0 ksi | ASTM D790 |
| Compressive Strength | 26.9 MPa | 3900 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 0.234 GPa | 34.0 ksi | ASTM D695 |
| Izod Impact, Notched | NB | NB | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
| Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Limited | Limited |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Machinability | 3 | 1-10, 1=Easier to Machine |