| Category | Polymer , Thermoplastic , Polyimide, Thermoplastic |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Duratron® PI |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Water Absorption | 0.70 % | 0.70 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 3.8 % | 3.8 % | ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 128 | 128 | ASTM D785 |
| Hardness, Shore D | 90 | 90 | ASTM D2240 |
| Tensile Strength | 121 MPa | 17500 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
| Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
| Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
| Compressive Strength | 186 MPa | 27000 psi | 10% Deformation; ASTM D695 |
| Compressive Modulus | 2.62 GPa | 380 ksi | ASTM D695 |
| Shear Strength | 110 MPa | 16000 psi | ASTM D732 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM 256 Type 'A' |
| Coefficient of Friction, Dynamic | 0.29 | 0.29 | Dry vs. Steel; QTM 55007 |
| K (wear) Factor | 302 x 10<sup>-8</sup> mm³/N-M | 150 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM55010 |
| Limiting Pressure Velocity | 0.525 MPa-m/sec | 15000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 40.5 µm/m-°C @Temperature -40.0 - 149 °C |
22.5 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Thermal Conductivity | 0.216 W/m-K | 1.50 BTU-in/hr-ft²-°F | ASTM E1530 |
| Melting Point | 304 °C | 580 °F | |
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 354 °C | 670 °F | ASTM D648 |
| Glass Transition Temp, Tg | 349 °C | 660 °F | ASTM D3418 |
| Flammability, UL94 | V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
| Dielectric Constant | 3.2 @Frequency 1.00e+6 Hz |
3.2 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.6 kV/mm | 395 kV/in | Short Term; ASTM D149 |
| Dissipation Factor | <= 0.0050 @Frequency 1.00e+6 Hz |
<= 0.0050 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |