| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Extruded |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Quadrant 1000 |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Quadrant 1000 LSP PC Extruded Unfilled Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Water Absorption | 0.20 % | 0.20 % | IMMERSION, 24 HRS. |
| Water Absorption at Saturation | 0.40 % | 0.40 % | ASTM D150 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
| Elongation at Break | 100 % | 100 % | ASTM D638 |
| Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
| Compressive Strength | 79.3 MPa @Strain 10.0 %, Temperature 22.8 °C |
11500 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D695 |
| Compressive Modulus | 2.07 GPa | 300 ksi | ASTM D695 |
| Shear Strength | 63.4 MPa | 9200 psi | ASTM D732 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.186 W/m-K | 1.29 BTU-in/hr-ft²-°F | |
| Glass Transition Temp, Tg | 145 °C | 293 °F | ASTM D 3418 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.17 | 3.17 | ASTM D150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
| Dissipation Factor | 0.00090 | 0.00090 | ASTM D150 |