| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Sanalite® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.920 g/cc | 0.920 g/cc | ASTM D792 |
| Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 78 | 78 | ASTM D2240 |
| Tensile Strength | 35.2 MPa | 5100 psi | ASTM D638 |
| Elongation at Break | 11 % | 11 % | ASTM D638 |
| Tensile Modulus | 1.31 GPa | 190 ksi | ASTM D638 |
| Flexural Strength | 35.2 MPa | 5100 psi | ASTM D790 |
| Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
| Compressive Strength | 37.9 MPa | 5500 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 1.38 GPa | 200 ksi | ASTM D695 |
| Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.25 | 0.25 | Dry vs. Steel; QTM55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | Yes | Yes | |
| FDA | Yes | Yes | |
| NSF | Yes | Yes | STD 2 & 51 |
| USDA | Yes | Yes | |
| USP Class VI | Yes | Yes |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Unacceptable | Unacceptable | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural | |
| Machinability | 3 | 1-10, 1=Easier to Machine |