Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Polypropylene - Calcium carbonate filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Reliance Industries
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
Flexural Strength 32.0 MPa
4640 psi
Flexural Modulus <= 2.90 GPa
<= 421 ksi
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F