| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
|
Nylene® 4121 (HS) Low Wear Nylon 6/6
Description: Nylene® 4121 (HS) is a high impact, low wear, 2% silicon oil reinforced nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting compani..
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE ZS506 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 TF10 Nylon 6.6 for injection molding, 10% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | FRISETTA Test Method |
|
Nilit RECONYL A H Recycled nylon 6.6 for injection molding
Recycled nylon 6.6 for injection molding, heat stabilized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | as molded; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **)
Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro..
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE Z606 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
|
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 K Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, formulated for the coloration of button baths.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
|
Reliance Industries Polypropylene - Calcium carbonate filled
Information provided by Reliance Industries
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
PolyOne Edgetek® NJ-000/000 Nylon 12
(discontinued **)
Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | |
|
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ASTM D955 |
|
Kolon KOPA® KN132VO Flame Retardant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO 2577 |
|
Polyram PlusTek PA340S05 Nylon 6.6 for Injection Molding, 5% Glass-beads Reinforced, Heat Stabilized
5% Glass-beads reinforced Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram.
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Tipco Tipcolene® FPTC 30 HG - 30% Talc & Calcium Carbonate Polypropylene Homopolymer, High Gloss & Stiffness
30% Talc+Calcium Reinforced PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO 294-4 |
|
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow
This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec
|
|||
| Linear Mold Shrinkage |
0.014
cm/cm <br>@Thickness 3.17 mm
|
0.014
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Diamond Polymers NYLON 6615 HS Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Linear Mold Shrinkage | 0.014 - 0.019 cm/cm | 0.014 - 0.019 in/in | ASTM D955 |
|
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable
Data provided by Clariant Masterbatches
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
|
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag..
|
|||
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
|
Ashley Polymers Ashlene® 279 PPO Alloy
A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid..
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | after bake; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 930HS TPO
(discontinued **)
Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
|
|||