Reliance Industries Repol H029SG Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol H029SG Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
REPOL Polypropylene H029SG is being manufactured using Unipol PP process, which combines the production efficiency of gas phase fluidized bed reactor with the high activity stereospecific catalyst system. Repol H029SG is recommended for use in Oriented Film process. Repol H029SG is the material of choice for BOPP films used in adhesive tapes, food packaging, cigarette & textile overwraps, lamination, synthetic paper etc.Features:High tensile strengthExcellent gloss and clarityGood processabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
50mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50mm/min; ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648