Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on tensile bar; SABIC Method
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 250 °C
30 g/10 min

@Load 11.0 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min; ISO 527
Flexural Strength 150 MPa
21800 psi
2 mm/min; ISO 178
Flexural Modulus 6.95 GPa
1010 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
3.40 J/cm²

@Temperature -30.0 °C
16.2 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 75

@Load 1.00 kg
75

@Load 2.20 lb
CS-17; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
47.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 173 °C
343 °F
Rate B/50; ISO 306
175 °C
347 °F
Rate B/120; ISO 306
UL RTI, Electrical 125 °C
257 °F
UL 746B
UL RTI, Mechanical with Impact 110 °C
230 °F
UL 746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
Glow Wire Test 960 °C

@Thickness 2.50 mm
1760 °F

@Thickness 0.0984 in
Glow Wire Flammability Index; IEC 60695-2-12
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
Users viewing this material also viewed the following: