Reltek BONDiT™ A-3 Bonding Agent, Primer and Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ A-3 Bonding Agent, Primer and Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Properties: Adhesion promoter and primer for coatings, sealants and adhesives on metals, glass and ceramic.Exceptional moisture and high pH resistance.Outstanding harsh environment protection and cathodic corrosion protection when used with the B-4811.Applications: Exceptional corrosion and chemical protection. Promotes adhesion and provides primer protection on most metals, ceramic and glass (including sapphire), most elastomers (including silicon) and low surface energy substrates. Functional for a wide range of overmold materials, paints, coatings, encapsulates. High thermal stability (250°C) and chemical resistance. Suitable for bonding semiconductor material. Used as adhesive for very thin bond lines (½ mil) such as for glass-to-glass and glass-to-polyethylene bonding. Compatible for use with BONDiT B-4X epoxy series. Ambient cure 60 min or accelerated thermal cure. Water white to slight amber.
Physical Properties Metric English Comments
Specific Gravity 1.018 - 1.038 g/cc
1.018 - 1.038 g/cc
ASTM D1298
Viscosity Measurement 4.5 - 8.5
4.5 - 8.5
ASTM D445
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Optical Properties Metric English Comments
Refractive Index 1.442 - 1.448
1.442 - 1.448
ASTM D1218
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 150 °C
0.0833 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color Clear with stray color