Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ritelok TL42 Nutlock

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok TL42 Nutlock.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Anaerobic. Medium strength threadlocker for screws, nuts and bolts. Prevent corrosion, Vibration resistant, Dismantle using normal tools
Physical Properties Metric English Comments
Viscosity 1200 - 5000 cP
1200 - 5000 cP
Mechanical Properties Metric English Comments
Impact Test 3.39 - 6.78 J
2.50 - 5.00 ft-lb
Torque Prevail
11.3 - 22.6 J
8.33 - 16.7 ft-lb
Torque Break
Descriptive Properties Value Comments
Maximum Bolt Size 0.635 - 1.91 cm
Users viewing this material also viewed the following: