| Category | Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Ethyl Cellulose, Molded |
| Manufacturer | Rotuba |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Rotuba 860S Ethyl Cellulose.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792-60T |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 96 | 96 | ASTM D785 |
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638-61T |
| Elongation at Break | 32 % | 32 % | ASTM D638-61T |
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256-56 |
| 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 137 °C | 279 °F | Flow temperature, ASTM D569-59 |
| Deflection Temperature at 0.46 MPa (66 psi) | 77.0 °C | 171 °F | ASTM D648-56 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.18 @Frequency 10000 Hz |
3.18 @Frequency 10000 Hz |
ASTM D150-54T |
| 3.23 @Frequency 1000 Hz |
3.23 @Frequency 1000 Hz |
ASTM D150-54T | |
| Dissipation Factor | 0.0072 @Frequency 1000 Hz |
0.0072 @Frequency 1000 Hz |
ASTM D150-54T |
| 0.0127 @Frequency 10000 Hz |
0.0127 @Frequency 10000 Hz |
ASTM D150-54T |