| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Lexan® LGN2000 PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.36 g/cc | 1.36 g/cc | ASTM D792 |
| Water Absorption | 0.16 % @Time 86400 sec |
0.16 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 91 | 91 | ASTM D785 |
| Tensile Strength, Yield | 86.0 MPa | 12500 psi | SABIC - Japan Method |
| Elongation at Break | 4.0 - 6.0 % | 4.0 - 6.0 % | SABIC - Japan Method |
| Flexural Strength | 147 MPa | 21300 psi | ASTM D790 |
| Flexural Modulus | 5.29 GPa | 767 ksi | ASTM D790 |
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 29.0 - 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 - 29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 148 °C @Thickness 3.20 mm |
298 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
UL 94 |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 3.2 @Frequency 50.0 - 60.0 Hz |
3.2 @Frequency 50.0 - 60.0 Hz |