Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SK Chemicals SKYTHANE® 395A S series Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SK Chemicals SKYTHANE® 395A S series Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Ultimate 55.9 MPa
8110 psi
ASTM D412
Tensile Strength, Yield 13.7 MPa

@Strain 100 %
1990 psi

@Strain 100 %
ASTM D412
29.4 MPa

@Strain 300 %
4270 psi

@Strain 300 %
ASTM D412
Elongation at Break 530 %
530 %
ASTM D412
Resilience 35
35
by vertical rebound; ASTM D2632
Tear Strength 157 kN/m
896 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 45
45
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525