Sanyo PELESTAT® 2450 Antistatic Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Sanyo Chemical Industries
Trade Name PELESTAT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sanyo PELESTAT® 2450 Antistatic Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) and give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a variety of thermoplastics like polyolefins, ABS, PC/ABS, PS, HIPS, Acetal Nylon, PBT, PTEG, etc. Pelestat® is not affected by moisture or humidity and offers the highest heat resistance of any anti-stats without affecting mechanical properties of the thermoplastic.Information provided by Tomen America, a US distributor of Pelestat.
Physical Properties Metric English Comments
Additive Loading 25 - 30 %
25 - 30 %
to achieve surface resistivity=10^11 ohms
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
Maximum Service Temperature, Air 280 °C
536 °F
Degradation Temp
Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
kept at 23°C under 50% R.H.
Descriptive Properties Value Comments
Appearance Pale Yellow Pellet
Applicable Thermoplastic PE