| Category | Polymer , Thermoplastic , Fluoropolymer , PFA , Polyperfluoroalkoxyethylene, Molded/Extruded |
| Manufacturer | ScanTube |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ScanTube PFA Tubing.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
| Water Absorption | <= 0.030 % | <= 0.030 % | ASTM D257 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 60 | 60 | ASTM D2240 |
| Tensile Strength | 27.6 MPa | 4000 psi | ASTM D638, ASTM D1708 |
| Elongation at Break | 300 % | 300 % | ASTM D638, ASTM D1708 |
| Tensile Modulus | 0.276 GPa | 40.0 ksi | ASTM D638 |
| Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
| Compressive Strength | 15.2 MPa | 2200 psi | ASTM D695 |
| Izod Impact, Notched | NB | NB | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.187 W/m-K | 1.30 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 305 °C | 581 °F | |
| Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
| Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 48.0 °C | 118 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | >= 95 % | >= 95 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.1 @Frequency 1000 Hz |
2.1 @Frequency 1000 Hz |
ASTM D150 |
| 2.1 @Frequency 1.00e+6 Hz |
2.1 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 78.7 kV/mm | 2000 kV/in | Short Term; 10 mil film; ASTM D149 |
| Dissipation Factor | 0.00020 @Frequency 1000 Hz |
0.00020 @Frequency 1000 Hz |
ASTM D150 |
| 0.00030 @Frequency 1.00e+6 Hz |
0.00030 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chemical Resistance | Excellent | |
| Weather Resistance | Excellent |