| Category | Ceramic , Glass , Optical , Filter |
| Manufacturer | Schott Glas Mainz |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott UG5 Band Pass Filter.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.85 g/cc | 0.103 lb/in³ |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 8.10 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.50 µin/in-°F @Temperature -22.0 - 158 °F |
|
| 9.40 µm/m-°C @Temperature 20.0 - 300 °C |
5.22 µin/in-°F @Temperature 68.0 - 572 °F |
||
| Transformation Temperature, Tg | 462 °C | 864 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.53 @Wavelength 1014 nm |
1.53 @Wavelength 1014 nm |
Hg |
| 1.54 @Wavelength 587.6 nm |
1.54 @Wavelength 587.6 nm |
He | |
| 1.56 @Wavelength 365 nm |
1.56 @Wavelength 365 nm |
Hg | |
| 1.60 @Wavelength 253.7 nm |
1.60 @Wavelength 253.7 nm |
Hg | |
| Transmission, Visible | <= 10 % @Wavelength 500 - 650 nm |
<= 10 % @Wavelength 500 - 650 nm |
|
| 66 % @Wavelength 690 nm |
66 % @Wavelength 690 nm |
Internal transmittance of 73% at 690 nm | |
| IR Transmittance | 76 % @Wavelength 720 nm |
76 % @Wavelength 720 nm |
Internal transmittance of 83% from 710-720 nm. |
| UV Transmittance | <= 6.0 % @Wavelength 200 - 220 nm |
<= 6.0 % @Wavelength 200 - 220 nm |
|
| 89 % @Wavelength 320 - 360 nm |
89 % @Wavelength 320 - 360 nm |
Internal transmittance of 98% from 320-360 nm | |
| Reflection Coefficient, Visible (0-1) | 0.91 | 0.91 |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 3 | 3 | |
| Alkali Class, AR | 2 | 2 | |
| Stain Resistance Class, FR | 0.0 | 0.0 |