Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinil Chemical SHINCON PPS-CF, Comp. "Y"-2 LCD Rack

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Shinil Chemical
Trade Name SHINCON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINCON PPS-CF, Comp. "Y"-2 LCD Rack.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since both materials cost high, there is a need to design the material with cost effectiveness. Also, the current LCD Rack has a concern of sloughing by CF particulates. SHINIL sloves these problems with the CNT composite of polyphenylene sulfide (PPS), polyether sulfone (PES), PEEK, or polyether imide (PEI) by providing the cost effectiveness combined with enhanced mechanical properties. Especially, the wear resistance (coefficient of friction, coefficient of abrasion) of SHINIL CNT composite was much lower than the current PEEK material, which will provide the material for clean/dust free LCD operation environments.Features and BenefitsPermanent electro conductivityImproved mechanical propertiesNo particulates and no sloughingLighter weightRecyclabilityLow abrasion and frictionImproved surfaceCost effectiveInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.4167

@Time 3600 sec,
Pressure 1.96 MPa
0.4167

@Time 1.00 hour,
Pressure 284 psi
0.2 m/s
Descriptive Properties Value Comments
Abrasion Weight (g) 0.0329
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr
Coefficient of Abrasion (10-3 cm2-sec/kgf-m-hr) 2.8206
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr
Users viewing this material also viewed the following: