Sibur MPP 21015-E10 Frost Resistant Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur MPP 21015-E10 Frost Resistant Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures
Physical Properties Metric English Comments
Melt Index of Compound 1.0 g/10 min
1.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 22.0 MPa
>= 3190 psi
Elongation at Break >= 200 %
>= 200 %
Charpy Impact Unnotched >= 5.00 J/cm²

@Temperature -50.0 °C
>= 23.8 ft-lb/in²

@Temperature -58.0 °F
Thermal Properties Metric English Comments
Vicat Softening Point >= 130 °C
>= 266 °F
10 hours at load
Descriptive Properties Value Comments
Frost Resistance <-40°C
For painted marks
<-50°C