Silberline SparkleBriteâ„¢ Premier 2052NL-PA

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name SparkleBrite™ Premier
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline SparkleBriteâ„¢ Premier 2052NL-PA.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SparkleBriteâ„¢ Premier pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced metallic effects in solvent and waterborne flexographic and gravure inks. The lenticular flake geometry produces strong, highly brilliant and very clean metallic effects. Although SparkleBriteâ„¢ Premier pigments can be used in aqueous inks they are not treated to protect against the aluminum-water reaction and special care must be taken to evaluate the gassing stability of each grade in the final ink formulation. High or excessive shear during ink production can initiate the aluminum-water reaction. Care must be taken to avoid excessive or high shear during processing when used in ink formulations containing water.Applications: Printing Inks
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
Volatiles 35 %
35 %
Particle Size 17 µm
17 µm
Descriptive Properties Value Comments
Category Non-leafing
Solvents Isopropyl Alcohol