Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Crosslinkable
Manufacturer Silon
Trade Name Taborex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLAS-SYSTEM”. It is used for the production of single and multi-layer pipes for domestic hot and cold water, under floor heating and central heating application.Information provided by Silon
Physical Properties Metric English Comments
Bulk Density 0.550 g/cc
0.0199 lb/in³
DIN 53466
Density 0.944 g/cc
0.0341 lb/in³
DIN 53479/ASTM D1505
Volatiles <= 0.10 %
<= 0.10 %
ITM-ZP 300CH 3-5-5/d
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133/ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 MPa
2760 psi
ISO R 527
Elongation at Break 250 %
250 %
ISO R 527
Processing Properties Metric English Comments
Zone 1 160 - 170 °C
320 - 338 °F
Zone 2 170 - 180 °C
338 - 356 °F
Zone 3 170 - 190 °C
338 - 374 °F
Zone 4 170 - 190 °C
338 - 374 °F
Die Temperature 190 - 220 °C
374 - 428 °F
Head Temperature 200 - 210 °C
392 - 410 °F
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Descriptive Properties Value Comments
Gel content (%) 71
EN 579
Users viewing this material also viewed the following: