| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.617 - 1.621 g/cc | 0.05842 - 0.05856 lb/in³ | D<sub>25/25</sub> |
| 1.474 g/cc @Temperature 110 °C |
0.05325 lb/in³ @Temperature 230 °F |
||
| 1.475 g/cc @Temperature 120 °C |
0.05329 lb/in³ @Temperature 248 °F |
||
| 1.49 g/cc @Temperature 100 °C |
0.0538 lb/in³ @Temperature 212 °F |
||
| 1.507 g/cc @Temperature 90.0 °C |
0.05444 lb/in³ @Temperature 194 °F |
||
| 1.523 g/cc @Temperature 80.0 °C |
0.05502 lb/in³ @Temperature 176 °F |
||
| 1.54 g/cc @Temperature 70.0 °C |
0.0556 lb/in³ @Temperature 158 °F |
||
| 1.557 g/cc @Temperature 60.0 °C |
0.05625 lb/in³ @Temperature 140 °F |
||
| 1.573 g/cc @Temperature 50.0 °C |
0.05683 lb/in³ @Temperature 122 °F |
||
| 1.59 g/cc @Temperature 40.0 °C |
0.0574 lb/in³ @Temperature 104 °F |
||
| 1.598 g/cc @Temperature 35.0 °C |
0.05773 lb/in³ @Temperature 95.0 °F |
||
| 1.606 g/cc @Temperature 30.0 °C |
0.05802 lb/in³ @Temperature 86.0 °F |
||
| 1.615 g/cc @Temperature 25.0 °C |
0.05835 lb/in³ @Temperature 77.0 °F |
||
| 1.623 g/cc @Temperature 20.0 °C |
0.05863 lb/in³ @Temperature 68.0 °F |
||
| 1.631 g/cc @Temperature 15.0 °C |
0.05892 lb/in³ @Temperature 59.0 °F |
||
| 1.64 g/cc @Temperature 10.0 °C |
0.0592 lb/in³ @Temperature 50.0 °F |
||
| 1.646 g/cc @Temperature 0.000 °C |
0.05947 lb/in³ @Temperature 32.0 °F |
||
| 1.648 g/cc @Temperature 5.00 °C |
0.05954 lb/in³ @Temperature 41.0 °F |
||
| Viscosity | 0.41 cP @Temperature 110 °C |
0.41 cP @Temperature 230 °F |
Dynamic |
| 0.44 cP @Temperature 100 °C |
0.44 cP @Temperature 212 °F |
Dynamic | |
| 0.48 cP @Temperature 90.0 °C |
0.48 cP @Temperature 194 °F |
Dynamic | |
| 0.51 cP @Temperature 80.0 °C |
0.51 cP @Temperature 176 °F |
Dynamic | |
| 0.56 cP @Temperature 70.0 °C |
0.56 cP @Temperature 158 °F |
Dynamic | |
| 0.61 cP @Temperature 60.0 °C |
0.61 cP @Temperature 140 °F |
Dynamic | |
| 0.66 cP @Temperature 50.0 °C |
0.66 cP @Temperature 122 °F |
Dynamic | |
| 0.68 cP @Temperature 120 °C |
0.68 cP @Temperature 248 °F |
Dynamic | |
| 0.73 cP @Temperature 40.0 °C |
0.73 cP @Temperature 104 °F |
Dynamic | |
| 0.76 cP @Temperature 35.0 °C |
0.76 cP @Temperature 95.0 °F |
Dynamic | |
| 0.80 cP @Temperature 30.0 °C |
0.80 cP @Temperature 86.0 °F |
Dynamic | |
| 0.84 cP @Temperature 25.0 °C |
0.84 cP @Temperature 77.0 °F |
Dynamic | |
| 0.89 cP @Temperature 20.0 °C |
0.89 cP @Temperature 68.0 °F |
Dynamic | |
| 0.94 cP @Temperature 15.0 °C |
0.94 cP @Temperature 59.0 °F |
Dynamic | |
| 0.99 cP @Temperature 10.0 °C |
0.99 cP @Temperature 50.0 °F |
Dynamic | |
| 1.05 cP @Temperature 5.00 °C |
1.05 cP @Temperature 41.0 °F |
Dynamic | |
| 1.11 cP @Temperature 0.000 °C |
1.11 cP @Temperature 32.0 °F |
Dynamic | |
| Molecular Weight | 165.8 g/mol | 165.8 g/mol | |
| Vapor Pressure | 0.00600 bar @Temperature 0.000 °C |
4.50 torr @Temperature 32.0 °F |
|
| 0.00800 bar @Temperature 5.00 °C |
6.00 torr @Temperature 41.0 °F |
||
| 0.0110 bar @Temperature 10.0 °C |
8.25 torr @Temperature 50.0 °F |
||
| 0.0140 bar @Temperature 15.0 °C |
10.5 torr @Temperature 59.0 °F |
||
| 0.0190 bar @Temperature 20.0 °C |
14.3 torr @Temperature 68.0 °F |
||
| 0.0250 bar @Temperature 25.0 °C |
18.8 torr @Temperature 77.0 °F |
||
| 0.0320 bar @Temperature 30.0 °C |
24.0 torr @Temperature 86.0 °F |
||
| 0.0410 bar @Temperature 35.0 °C |
30.8 torr @Temperature 95.0 °F |
||
| 0.0530 bar @Temperature 40.0 °C |
39.8 torr @Temperature 104 °F |
||
| 0.0830 bar @Temperature 50.0 °C |
62.3 torr @Temperature 122 °F |
||
| 0.128 bar @Temperature 60.0 °C |
96.0 torr @Temperature 140 °F |
||
| 0.190 bar @Temperature 70.0 °C |
143 torr @Temperature 158 °F |
||
| 0.275 bar @Temperature 80.0 °C |
206 torr @Temperature 176 °F |
||
| 0.389 bar @Temperature 90.0 °C |
292 torr @Temperature 194 °F |
||
| 0.540 bar @Temperature 100 °C |
405 torr @Temperature 212 °F |
||
| 0.733 bar @Temperature 110 °C |
550 torr @Temperature 230 °F |
||
| 0.979 bar @Temperature 120 °C |
734 torr @Temperature 248 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 0.840 J/g-°C @Temperature 0.000 °C |
0.201 BTU/lb-°F @Temperature 32.0 °F |
|
| 0.850 J/g-°C @Temperature 20.0 °C |
0.203 BTU/lb-°F @Temperature 68.0 °F |
||
| 0.870 J/g-°C @Temperature 40.0 °C |
0.208 BTU/lb-°F @Temperature 104 °F |
||
| 0.880 J/g-°C @Temperature 60.0 °C |
0.210 BTU/lb-°F @Temperature 140 °F |
||
| 0.900 J/g-°C @Temperature 80.0 °C |
0.215 BTU/lb-°F @Temperature 176 °F |
||
| 0.910 J/g-°C @Temperature 100 °C |
0.217 BTU/lb-°F @Temperature 212 °F |
||
| 0.930 J/g-°C @Temperature 120 °C |
0.222 BTU/lb-°F @Temperature 248 °F |
||
| Distillation Temperature | 110.6 - 121.6 °C | 231.1 - 250.9 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear without suspended matter | ASMT D3741/B |
| Color | <10 | APHA |
| Composition | <1 mg/kg | Chlorides (Cl) |
| <10 mg/kg | Additive (Stabilizer) | |
| <10 mg/kg | Non volatile Residue | |
| <15 mg/kg | Organically combined Oxygen and Nitrogen | |
| <25 mg/kg | Moisture (H2O), Karl Fischer, ASTM E1064 | |
| Purity | >999.5 g/kg | without stabilizers |