Solvay Engineered Polymers SEQUEL® 1492 Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1492 Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: SEQUEL® 1492 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent processability. This product is designed for pre-colored, unpainted applications. Applications: Bumper fascias and other large components that must exhibit durable paintability or excellent weatherability. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
as molded; ISO 294
Melt Flow 28 g/10 min
28 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.8 MPa
3020 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.60 GPa
232 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test >= 29.4 J
>= 21.7 ft-lb
multiaxial, 2.2 m/s; ASTM D3763