Solvay Specialty Polymers Algoflon® 55BZ+5Mos PTFE; Bronze/Molybdenum Disulphide Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Algoflon® 55BZ+5Mos PTFE; Bronze/Molybdenum Disulphide Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.55 wt.% Bronze + 5 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 3.88 g/cc
0.140 lb/in³
ASTM D792
Apparent Bulk Density 0.960 g/cc
0.0347 lb/in³
ASTM D4894
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C

@Temperature 23.0 - 250 °C
77.8 µin/in-°F

@Temperature 73.4 - 482 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service