Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Royalstatâ„¢ R635 ABS/Polyolefin Static Control Sheet

Category Polymer , Thermoplastic , ABS Polymer , Polyolefin
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalstatâ„¢ R635 ABS/Polyolefin Static Control Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Static Control SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
ASTM D785
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Flexural Yield Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Falling Dart Impact 271 J

@Temperature -40.0 °C
200 ft-lb

@Temperature -40.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+05
<= 1e+05
ASTM D257