Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals Nitinol Chrome-Doped Superelastic Ni-Ti alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy , Titanium Alloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name Nitinol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals Nitinol Chrome-Doped Superelastic Ni-Ti alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology.
Physical Properties Metric English Comments
Density 6.50 g/cc
0.235 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1550 MPa
>= 225000 psi
Elongation at Break 8.0 %
8.0 %
max strain recovery
>= 10 %
>= 10 %
Tensile Set 0.10 %
0.10 %
permanent set after 6% strain
Thermal Properties Metric English Comments
Melting Point 1300 °C
2370 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 0.20 - 0.30 %
0.20 - 0.30 %
Hydrogen, H <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.050 %
<= 0.050 %
Nickel, Ni 55.3 - 56.3 %
55.3 - 56.3 %
Oxygen, O <= 0.050 %
<= 0.050 %
Titanium, Ti 43.235 - 44.5 %
43.235 - 44.5 %
Descriptive Properties Value Comments
Lower superelastic plateau stress, ksi 35
Upper superelastic plateau stress, ksi 80