Sylvin Technologies 9077-70 Natural PVC for Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9077-70 Natural PVC for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Thickness 1000 microns
39.4 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 seconds
Tensile Strength, Ultimate 7.58 MPa
1100 psi
Elongation at Break 310 %
310 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
RTI
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 160 - 171 °C
320 - 340 °F