Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Melt Temperature 160 - 171 °C
320 - 340 °F
PolyOne Geon™ Vinyl Wire & Cable 0650-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 160 - 180 °C
320 - 356 °F
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Melt Temperature 160 - 180 °C
320 - 356 °F
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Melt Temperature 160 - 165 °C
320 - 329 °F
ASTM D789
Niche Polymer PPHM15BK Homopolymer PP
Information provided by Niche Polymer
Melt Temperature 160 - 218 °C
320 - 424 °F
Injection
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced  (discontinued **)
Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: Flame Retardant: Balance of Properties (Impact, Mechanical and Heat)Applications: Computer, Monitor and Printer Housings, Microwave Co..
Melt Temperature 160 - 166 °C
320 - 331 °F
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 160 - 205 °C
320 - 401 °F
NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided..
Melt Temperature 160 - 207 °C
320 - 405 °F
Average value: 188 °C Grade Count:25
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Melt Temperature 160 °C
320 °F
LyondellBasell Petrothene® M2520FN Low Density Polyethylene
ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory..
Melt Temperature 160 - 180 °C
320 - 356 °F
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene
LF0200 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. LF0200 contains antioxidant.Applications: genera..
Melt Temperature 160 - 180 °C
320 - 356 °F
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene
LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Melt Temperature 160 - 220 °C
320 - 428 °F
Lucobit Lucobit® 1220 Ethylene Copolymer Bitumen
Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci..
Melt Temperature 160 - 220 °C
320 - 428 °F
Lucobit Lucofin® 1461 Polyolefin TPO Granules, Ice Blue
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Melt Temperature 160 - 180 °C
320 - 356 °F
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene
LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Melt Temperature 160 - 180 °C
320 - 356 °F
Lucobit Lucofin® 1413-t1 Polyolefin TPO Granules, Dark Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..
Melt Temperature 160 - 171 °C
320 - 340 °F
Sylvin Technologies 8940-70 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 160 - 171 °C
320 - 340 °F
Sylvin Technologies 8999-70 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 160 - 171 °C
320 - 340 °F
Sylvin Technologies 9925-70 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Melt Temperature 160 °C
320 °F
Teknor Apex APEX® 3200-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Melt Temperature 160 °C
320 °F
Teknor Apex APEX® 3210-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Melt Temperature 160 °C
320 °F
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t..
Melt Temperature 160 °C
320 °F
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic..
Melt Temperature 160 °C
320 °F
A. Schulman PP 3489-01 Polypropylene Homopolymer
DescriptionPolypropylene PP 3489-01 is a specially designed homopolymer with excellent stiffness properties. ApplicationTypical applications include high speed extrusion, high speed thin wall injec..
Melt Temperature 160 °C
320 °F
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for..
Melt Temperature 160 - 185 °C
320 - 365 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Melt Temperature 160 °C
320 °F
Axiall 50897 Moldings & Extrusions Flexible PVC
Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 160 - 230 °C
320 - 446 °F
Average value: 190 °C Grade Count:8
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Melt Temperature 160 - 166 °C
320 - 331 °F
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Melt Temperature 160 - 180 °C
320 - 356 °F
Lucobit Lucofin® 1412-t1 Polyolefin TPO Granules, Light Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..
Melt Temperature 160 - 205 °C
320 - 401 °F
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin  (discontinued **)
Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer.