Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMCAL TIMREX® SFG150 Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® SFG150 Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Tribological and mechanical properties:Low toughnessGood lubrication propertiesAdvantages and applications: Very low friction coefficientLow wear of the counterpartExtreme good formation of transfer-filmVery high electrical conductivityExcellent wettability with organic binders Excellent compressibilityHigh transverse rupture strengthsuitable for pitch-bonded, resin-bonded and metallic brushes Information provided by TIMCAL
Physical Properties Metric English Comments
Oil Absorption 45 %
45 %
wt %, DBP, 140 um particle size
Particle Size 5.0 µm
5.0 µm
Springback 8%, pressure 0.477 t/cc
5.0 µm
5.0 µm
at a density of 1.90 g/cc, pressure 2.5 t/cc
10 µm
10 µm
at a density of 1.92 g/cc, pressure 2.5 t/cc
42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
75 µm
75 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
75 µm
75 µm
Springback 6.5%, pressure 0.477 t/cc
Specific Surface Area 2.5 m²/g
2.5 m²/g
BET
Ash 0.030 %
0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.750 ohm-cm
0.750 ohm-cm
particle size 75 um, pressure 2.5 t/cc
0.800 ohm-cm
0.800 ohm-cm
particle size 40 um, pressure 2.5 t/cc
1.45 ohm-cm
1.45 ohm-cm
particle size 15 um, pressure 2.5 t/cc
1.75 ohm-cm
1.75 ohm-cm
particle size 10 um, pressure 2.5 t/cc
Processing Properties Metric English Comments
Moisture Content 0.010 %
0.010 %
Descriptive Properties Value Comments
Crystallinity Height Lc >200 nm