Material Notes:
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 89
85 - 89
Tensile Strength 29.4 MPa
4270 psi
Elongation at Break 600 %
600 %
100% Modulus 0.00490 GPa
0.710 ksi
300% Modulus 0.00883 GPa
1.28 ksi
Processing Properties Metric English Comments
Processing Temperature 165 - 200 °C
329 - 392 °F