| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 193 MPa | 28000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
| Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 254 °C | 490 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |