Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm

@Thickness 3.17 mm
0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 91.7 MPa
13300 psi
ASTM D790
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.4 µm/m-°C
23.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
215 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 18.9 kV/mm
480 kV/in
Method A (Short-Time); ASTM D149