Teknor Apex Tekbond® TB 1372A Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name TEKBOND®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Tekbond® TB 1372A Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, but also create a novel tactile and aesthetic experience. Tekbond® TPEs enable insert and 2-shot molding production of hybrid parts requiring distinctive functional and aesthetic performance criteria and marketing appeal, often at substantially reduced finished cost. Designer engineers have been selecting Tekbond® TPE to replace the more expensive and higher density TPUs. Tekbond® applications include hand held electronics and industrial diagnostic devices, lawn & garden and power tools. Special Characteristic: Low FlowInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength 7.93 MPa
1150 psi
Elongation at Break 300 %
300 %