Material Notes:
Radical polyethylene made by high pressure autoclave process. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.0 MPa
2030 psi
ISO R527
Tensile Strength, Yield 12.0 MPa
1740 psi
ISO R527
Elongation at Break 650 %
650 %
ISO R527
Modulus of Elasticity 0.240 GPa
34.8 ksi
ISO 5527
Dart Drop Test 190 g
0.419 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 114 °C
237 °F
ISO 11357-3
Vicat Softening Point 98.0 °C
208 °F
ISO 306
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
50µ; ASTM D 1003
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.