UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=5)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=5).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE.
Physical Properties Metric English Comments
Fiber Count 1520 dtex
1370 denier
Mechanical Properties Metric English Comments
Elongation at Break 27 %
27 %
Line Elongation
27 %
27 %
Knot Elongation
Tenacity 0.424 N/tex
4.80 g/denier
Knot Strength
0.697 N/tex
7.90 g/denier
Line Strength
2.03 N/tex
23.0 g/denier
Tensile Modulus