UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplications: Small- large size sport fishing line and long line (branch line), Appearance of filament is said to be "brilliant crystal tone" and reputed in the branch line applicationInformation provided by UBE.
Physical Properties Metric English Comments
Fiber Count 1510 dtex
1360 denier
Mechanical Properties Metric English Comments
Elongation at Break 27 %
27 %
Knot Elongation
31 %
31 %
Line Elongation
Tenacity 0.671 N/tex
7.60 g/denier
Knot Strength
0.777 N/tex
8.80 g/denier
Line Strength
1.94 N/tex
22.0 g/denier
Tensile Modulus
Thermal Properties Metric English Comments
Shrinkage 21 %
21 %