| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Ravago Manufacturing Americas, LLC |
| Trade Name | Hylon® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | DAM; ASTM D792 |
| Water Absorption | 1.2 % | 1.2 % | 24 hrs, DAM; ASTM D570 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | 0.125 in, DAM; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | 73°F; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | HB | HB | 0.0590 in, BK |
| HB | HB | 0.0590 in, NC |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
| Drying Temperature | 73.9 °C | 165 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | 0.18 % | 0.18 % | |
| Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
| Screw Speed | 50 - 120 rpm | 50 - 120 rpm |