Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
ASTM D412
Tensile Strength at Break 18.1 MPa
2630 psi
ASTM D412
Elongation at Break 530 %
530 %
ASTM D412
100% Modulus 0.00200 GPa
0.290 ksi
ASTM D412
200% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
300% Modulus 0.00920 GPa
1.33 ksi
ASTM D412
Tear Strength 41.0 kN/m
234 pli
ASTM D2240