Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Network Polymers Softflex® 2701T Transparent Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® PS455-200 TPU-Polyester Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-360A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 527 |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 3004-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3004-111 is specifically designe.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Black, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Natural, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Natural, Halogen Free Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R Highly Extended Low-Cost Hose FormulationNordel® IP 4770R |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600550S SEBS Based Material, Filled Qualities, 55A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D 638 |
API Megol AM DP2217/60PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00200 - 0.0120 GPa | 0.290 - 1.74 ksi | |
Dow Advanta® 3302 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |
|||
100% Modulus | 0.00200 - 0.0120 GPa | 0.290 - 1.74 ksi | |
Dow Advanta® 3650 Specialty Elastomer