Universal Wire Works 141 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 141 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 141 (Eni-1) is used for welding Nickel 200 and 201 to themselves or to one another, for overlaying on steel, or welding on the clad side of steel clad with nickel. Typical applications include welding ASTM B160, B161, B162, and B163. Dissimilar metal welding applications are: joints between Nickel 200 and 201 and a variety of iron-base and nickel-base alloys. Alloy 141 in the 3/32 and 1/8 diameters can be used in all positions, while the larger 5/32 and 3/16 diameter are used in the flat and horizontal positions. POWER SUPPLY DCRP.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 414 MPa
60000 psi
Elongation at Break 20 %
20 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.0 %
<= 1.0 %
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 0.80 %
<= 0.80 %
Manganese, Mn <= 0.75 %
<= 0.75 %
Nickel, Ni >= 92 %
>= 92 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 1.25 %
<= 1.25 %
Sulfur, S <= 0.020 %
<= 0.020 %
Titanium, Ti 1.0 - 4.0 %
1.0 - 4.0 %